Wear Protection Methods for Vapour Turbine Blades
This article presents a literature review of methods for protecting steam turbine blade surfaces from wear in order to extend their service life. The analysis concludes that the main causes of blade damage are erosion-corrosion processes and the effect of elevated temperatures inside the turbine. Progressive wear reduces the efficiency and power output of the entire power unit. The most common methods used to protect blade surfaces from wear are: surface hardening, application of protective overlays, spraying of protective coatings, generation of layers by laser surfacing and shot peening of blade surfaces. The use of surface protection against wear extends the service life of the turbine, reducing the cost and time-consuming repair work.
W artykule przedstawiono przegląd literatury dotyczącej metod zabezpieczania powierzchni łopat turbin parowych przed zużyciem w celu wydłużenia czasu ich eksploatacji. W wyniku przeprowadzonej analizy stwierdzono, że głównymi przyczynami uszkodzenia łopat są procesy erozyjno-korozyjne oraz wpływ podwyższonej temperatury wewnątrz turbiny. Postępujące zużycie zmniejsza sprawność i moc całego bloku energetycznego. Najczęściej stosowane metody zabezpieczenia powierzchni łopat przed zużyciem to: hartowanie powierzchniowe, zastosowanie nakładek ochronnych, natryskiwanie powłok ochronnych, wytwarzanie warstw przez napawanie laserowe oraz kulowanie powierzchni łopat. Zastosowanie zabezpieczenia powierzchni przed zużyciem wydłuża czas pracy turbiny, ograniczając koszt i czasochłonność prac naprawczych.
Opracowanie rekordu ze środków MNiSW, umowa nr POPUL/SP/0154/2024/02 w ramach programu "Społeczna odpowiedzialność nauki II" - moduł: Popularyzacja nauki (2025).