Anomalous leakage currents on silicone rubber hollow insulators
Leakage currents on silicone and porcelain housings were measured at a 110 kV substation (site pollution severity class heavy) for 7 months. Both types of housing had a similar geometry. The current on porcelain housings is usually up to 4,7 times higher than on silicone housings. However, significantly smaller currents (up to 2,6 times) were recorded on the porcelain insulators over a period of 8 days. Similar rare behavior was earlier seen at Glogow pollution test station and at Koeberg pollution test station on porcelain and silicone insulators with the same profiles. A better washability of porcelain during stronger rains plays a very important role in this phenomenon. It was shown that small leakage currents, usually in the range 4 -10 mA, cause surface erosion of silicone rubber housings.
Przez 7 miesięcy mierzono prąd upływu na osłonach silikonowych I porcelanowych na rozdzielni 110 kV znajdującej się w III strefie zabrudzeniowej). Osłony miały podobny kształt. Prąd na osłonie porcelanowej był zazwyczaj większy niż na osłonie silikonowej (do 4,7 razy). Jednakże w ciągu 8 dni prąd na osłonie porcelanowej był mniejszy (do 2, 6 razy). Podobne takie rzadkie przypadki zauważono wcześniej na stacjach zabrudzeniowych w Koeberg i w Hucie Głogów na izolatorach o identycznym kształcie. Bardzo ważną rolę w tym zjawisku odgrywa lepsze oczyszczanie porcelany przez silniejsze deszcze. Wykazano, że niewielkie prądy upływu rzędu 4 –10 mA powodują erozję powierzchniową osłon silikonowych.
Opracowanie rekordu ze środków MNiSW, umowa Nr 461252 w ramach programu "Społeczna odpowiedzialność nauki" - moduł: Popularyzacja nauki i promocja sportu (2020).