Tytuł pozycji:
Beneficiation of Egyptian Abu-Swayel copper ore by flotation
In this study, an attempt was made to recover copper from Abu-Swayel deposit. A reverse flotation technique was applied leading to flotation of the accompanying oxide and sulfide minerals and gathering copper oxide minerals in the sink product. The results showed that the application of such technique is possible under the optimum flotation conditions. Studying the main factors that affect such flotation system indicated that the optimum flotation conditions are at 1.5 kg/t oleic acid as the collector, pH=10, air flow rate=7 1/min and 5 min flotation time. In the context, about 90% of copper recovery with 10% copper grade was obtained. It was also found that the copper mineral particles lost in the froth product by mechanical carryover mechanism can be recovered through concentrate cleaning under the same flotation conditions. Hence, one may conclude that the results of this study are useful and may help in reassessment of exploitation of such copper deposit.
W pracy podjęto próbę odzysku miedzi z egipskiego złoSa Abu-Swayel. Zastosowano flotację odwrotną polegającą na flotacji towarzyszących tlenków i siarczków, gromadząc minerały tlenkowe miedzi w produkcie tonącym. Stwierdzono, Se technika ta jest uSyteczna, ale w warunkach optymalnych. Badania głównych czynników wpływających na stosowany układ flotacyjny wskazują, Se optymalne warunki flotacji to 1.5 kg/Mg kwasu oleinowego jako kolektora, pH=10, przepływ powietrza 7 dm3/min a czas flotacji to 5 minut. W tych warunkach otrzymano 10% koncentraty miedziowe przy uzysku około 90%. Stwierdzono takSe, iS ziarna minerałów miedzi stracone w produkcie pianowym są wynoszone mechanicznie i mogą być odzyskiwane przez czyszczenie koncentratu w tych samych warunkach flotacji. MoSna zatem powiedzieć, Se wyniki tych badań są pozytywne i mogą pomóc przy ponownej ocenie moSliwości eksploatacji złóS miedziowych tego typu.